Description
FURNACE MIX +1700 0C
USAGE
For laying chamotte brick furnaces
COMPOSITION
Fine-grained chamotte fraction (over 95%) and other heat-resistant additives.
TECHNICAL SPECIFICATION
Furnace mix fraction below 0.2 mm.
Fire resistance of the furnace mix +1700 0C.
Consumption rate of dry mix per chamotte brick approximately 0.2 kg.
PREPARATIONS
Pour the required quantity of the dry mix in the mixing bowl or mixer.
Add water 25-27% of the mix weight.
Stir mechanically or manually until the mix is completely wet.
The ready mix resembles grainy pasta.
Usage time of ready mix: up to 4 hours.
APPLICATION
Minimum working temperature + 5 0C.
Furnace mix thickness between chamotte bricks should be 2-3 mm.
The mix cures and forms a bond between bricks in a couple of hours.
STORAGE
Mix powder should be stored in its original package in a dry room.
Shelf life of the mix in an unopened original package is 12 months from the manufacturing date.